Production of the coolant ducts by pressing. Cylindrical, prismatic and other sections. Coolant ducts
1-fold – 5-fold
central
parallel
spiralised
Shaping: turning, milling, sawing
The chalk-like-texture of the green part allows the inserting of complex geometries before the sinter process.
Sintering: Pressure, Temperature, Time, Experience
We are sintering your parts by continuous operation in eight sinter furnaces at temperatures of more than 1300 °C. Our experience of long duration assures the continuity of the Gühring-Quality.
Wire eroding
Die sinking and wire eroding for the reworking.
Analysis
Quality management as the symbol of our claim: metallography, analysis of the carbide grade, magnetism, density, hardness.
Examination
Dimensional check, concentric run-out, ultrasonic sound, coolant ducts, acoustics. The quality of our products is a priority. Each order will be checked. A high degree of automation for more efficiency.
Grinding
To refine your previously produced blank optionally, we grind it at one of our many grinders.